Home > Inorganic Salts >

LiFOB Electrolyte Additives CAS NO 409071-16-5 99.9%

Categories Electrolyte Additives
Certification: ISO9001
Place of Origin: China
MOQ: 1g
Price: negotiation
Payment Terms: TT
Supply Ability: 10Ton/Month
Delivery Time: This is advantaged product, we have it in stock.
Packaging Details: bottle/drum/bag
Brand Name: Yacoo
Model Number: E0523
CAS: 409071-16-5
Assay: 99.9%
Formula: C2BF2LiO4
Appearance: White powder
MP: 265-271℃
Storage: Preserve in a well-closed container and keep in cool, dry place
  • Product Details
  • Company Profile

LiFOB Electrolyte Additives CAS NO 409071-16-5 99.9%

Quick Detail:


Name

Lithium Difluoro(oxalato)borate

Appearance

White powder

Assay:

≥99.9

Iron,ppm

≤5

Water content,ppm

≤500

potassium, ppm

≤10


Description:

> Formula: C2BF2LiO4

> Weight: 143.77

> Appearance: White powder

> MP:265-271℃(MP)

>Storage: Preserve in a well-closed container and keep in cool, dry place

> Danger Description:

> Safety Description:

> Danger Symbol:

> Shelf life:two years


1.Applications:

A.Nonaqueous electrolyte compositions

B.Non-aqueous electrolyte for lithium-​ion battery

2.Location

A. biology/biochemistry laboratory, pharmaceutical factory, cosmetics factory


Specifications

Assay

≥99.9

Chlorine,Calcium and Sodium,ppm

≤10

Water content,ppm

≤500

Nickel,ppm

≤50


Synonyms:

Lithium difluoro(oxalato)borate;Lithium difluoro(oxalato)borate(1-);LithiuM Oxalyldifluoroborate


The determination of KF

Use MA-1 intelligent Carle Fischer moisture tester to measure water content


Determination of melting point

Instrument:

Micro melting point apparatus WRS-2A, Melting point tubes

Determination of step:

Open switch, stable 20min.

First set the starting temperature than the melting point of the low 10 ℃, heating rate 2 ℃ / min.

The sample was grind as fine as possible and load in a clean, dry melting point pipe ,until the sample was compressed into about 1cm high .When the actual temperature reaches the set temperature and stabilized . Inserted into the capillary with the sample, the simultaneous determination of three.


Determination of iron content

Preparation of standard iron solution

Weigh ammonium iron(III) sulfate [FeNH4(SO4)2·12H2O] 0.863g .Placed in 1000mL volumetric flask, add water to dissolveand add sulfuric acid 2.5mL.Diluted with water to the mark, shake, as the stock solution.

Before use, exact amount of stock solution 1mL, placed in 100mL flask, diluted with water to the mark and shake.

Weigh 1g sample, placed in a crucible.Adding sodium carbonate 2g and mixed.Burning at 740 ℃,the residue is dissolved in dilute hydrochloric acid 15ml , displacing 50mL Nessler colorimetric tube , add dilute hydrochloric acid 4mL and ammonium persulfate 50mg , Diluted with water to make into 35mL, add 30% ammonium thiocyanate solution 3mL, plus the amount of water diluted into 50mL, shaked. If the color, take 1mL standard iron solution into 50mL Nessler colorimetric tube, add water to 25mL,4mL dilute hydrochloric acid and 50mg ammonium persulfate , diluted with water to 35mL, then plus 30% ammonium thiocyanate solution 3mL, plus the amount of water diluted into 50mL, shake comparisons.

Product Tags:

EDOT

  

Electrochemical materials

  
Cheap LiFOB     Electrolyte Additives  CAS NO     409071-16-5     99.9% for sale
Send your message to this supplier
 
From:
To: Suzhou yacoo chemical reagent corporation
Subject:
Message:
Characters Remaining: (0/3000)
 
You may also be interested in :
Inquiry Cart 0
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
  • Submit Buying Request
    Contact Us Quickly